✍️ 🧑‍🦱 💚 Autor:innen verdienen bei uns doppelt. Dank euch haben sie so schon 472.549 € mehr verdient. → Mehr erfahren 💪 📚 🙏

NANOINDENTATION STUDY ON NiTi THIN FILM SHAPE MEMORY ALLOYS

NANOINDENTATION STUDY ON NiTi THIN FILM SHAPE MEMORY ALLOYS

von Ajit Behera und Pratik Mohanty
Softcover - 9786202679671
39,90 €
  • Versandkostenfrei
Auf meine Merkliste
  • Hinweis: Print on Demand. Lieferbar in 2 Tagen.
  • Lieferzeit nach Versand: ca. 1-2 Tage
  • inkl. MwSt. & Versandkosten (innerhalb Deutschlands)

Autorenfreundlich Bücher kaufen?!

Beschreibung

A single bi-layered sample consisting of a monolayer of Ni and a monolayer of Ti with the Ni layer as a base layer was deposited on a silicon substrate. During deposition, the substrate was rotated at a predefined speed. The as deposited layers were then annealed at temperatures of 300 ¿ C, 400 ¿ C,500 ¿ C and 600 ¿ C, for a time period of 1 hour in a vacuum furnace in order to achieve crystallinity in the as deposited layers and form a crystalline single layer and also for the purpose of chemical homogeneity. The thesis deals with the process of manufacture of NiTi thin film shape memory alloys and the characterisation of their morphology as well as the mechanical properties of the thin films like hardness, reduced elastic modulus and hence the elastic modulus, wear rate and hence the wear resistance, depth recovery ratio and consequently the super elastic properties. The films were manufactured in a DC/RF magnetron sputtering machine on thoroughly cleaned Si substrate held at a temperature of 300 ¿ C from two 99.99 % pure 75 mm Ni and Ti target materials in an inert atmosphere made up of 99.99% pure Argon. During deposition, the substrate was rotated at a predefined speed. Tot

VARYING ANNEALING TEMPERATURE

Details

Verlag LAP LAMBERT Academic Publishing
Ersterscheinung 15. Juli 2020
Maße 22 cm x 15 cm x 0.5 cm
Gewicht 107 Gramm
Format Softcover
ISBN-13 9786202679671
Seiten 60