✍️ 🧑‍🦱 💚 Autor:innen verdienen bei uns doppelt. Dank euch haben sie so schon 486.154 € mehr verdient. → Mehr erfahren 💪 📚 🙏

Mechanical properties of carbon nitride coatings by nanoindentation technique

Mechanical properties of carbon nitride coatings by nanoindentation technique

von Vikrant Dev Rathore
Softcover - 9783346165626
27,95 €
  • Versandkostenfrei
Auf meine Merkliste
  • Hinweis: Print on Demand. Lieferbar in 2 Tagen.
  • Lieferzeit nach Versand: ca. 1-2 Tage
  • inkl. MwSt. & Versandkosten (innerhalb Deutschlands)

Autorenfreundlich Bücher kaufen?!

Beschreibung

Bachelor Thesis from the year 2018 in the subject Engineering - Mechanical Engineering, grade: 10/10, Panjab University (CSIR-National Physical Laboratory), course: Mechanical Engineering, language: English, abstract: Carbon Steel Rings Used in the textile industries lack the robust qualities required and thus a suitable coating was required to enhance their mechanical properties. The Properties of carbon Steel (uncoated) and coated with carbon nitride were studied using Nanoindentation. Furthermore for the coated samples uncertainty in Nanoindentation was evaluated and taken into account.

This training report gives a brief introduction to Nanoindentation and its wide range of applications along with uncertainty analysis of mechanical properties that might be present during the Nanoindentation process. The uncertainty analysis also shows that Nanoindentation is an effective technique in determining the mechanical properties of carbon nitride coated samples. Not only does the carbon nitride coating improve mechanical properties like hardness and reduced modulus but also adds aesthetic features as well to the carbon steel sample.

Details

Verlag GRIN Verlag
Ersterscheinung 15. Juni 2020
Maße 21 cm x 14.8 cm x 0.5 cm
Gewicht 107 Gramm
Format Softcover
ISBN-13 9783346165626
Auflage 1. Auflage
Seiten 64

Schlagwörter