✍️ 🧑‍🦱 💚 Autor:innen verdienen bei uns doppelt. Dank euch haben sie so schon 476.753 € mehr verdient. → Mehr erfahren 💪 📚 🙏

Stress Corrosion Cracking of X-70 steel in  carbonates, solutions

Stress Corrosion Cracking of X-70 steel in carbonates, solutions

von Alvaro Torres, Bernardo Campillo und Sergio Serna
Softcover - 9783846534717
49,00 €
  • Versandkostenfrei
Auf meine Merkliste
  • Hinweis: Print on Demand. Lieferbar in 2 Tagen.
  • Lieferzeit nach Versand: ca. 1-2 Tage
  • inkl. MwSt. & Versandkosten (innerhalb Deutschlands)

Autorenfreundlich Bücher kaufen?!

Beschreibung

The aim of this work was to study the effect of different heat treatments on the stress corrosion cracking (SCC) resistance of X-70 pipeline steel in diluted solutions of NaHCO3 (0.1 M, 0.05 M, 0.01 M, and 0.005 M), and in solutions of NaHCO3 with addition of KCl, CaCl2 and MgSO4-7H2O, using the slow strain rate testing (SSRT) technique,and some heat treatments.The results obtained indicated that the quenched and quenched+tempered conditions are the only ones susceptible to HE and the mechanism of SCC in X-70 pipeline steel increased in most diluted solution of NaHCO3 at 50¿C, and was dominated by film rupture an anodic dissolution.

Stress Corrosion Cracking of X-70 Microalloyed steel in carbonates, chlorides and sulfates solutions

Details

Verlag LAP LAMBERT Academic Publishing
Ersterscheinung 18. Oktober 2011
Maße 22 cm x 15 cm x 0.5 cm
Gewicht 107 Gramm
Format Softcover
ISBN-13 9783846534717
Seiten 60