{"product_id":"stress-corrosion-cracking-of-x-70-steel-in-carbonates-solutions-von-alvaro-torres-sergio-serna-und-bernardo-campillo","title":"Stress Corrosion Cracking of X-70 steel in  carbonates, solutions","description":"\u003cp\u003eThe aim of this work was to study the effect of different  heat treatments on the stress corrosion cracking (SCC) resistance of X-70 pipeline steel  in diluted solutions of NaHCO3 (0.1 M, 0.05 M, 0.01 M, and 0.005 M), and in solutions of NaHCO3 with addition of KCl, CaCl2 and MgSO4-7H2O, using the slow strain rate testing (SSRT) technique,and  some  heat treatments.The results obtained indicated that the quenched and quenched+tempered conditions are the only ones susceptible to HE and the mechanism of SCC in X-70 pipeline steel increased in most diluted solution of NaHCO3 at 50¿C, and was dominated by film rupture an anodic dissolution.\u003c\/p\u003e\u003cdiv class=\"aw-variant-hidden-subtitle-div\" id=\"aw-variant-subtitle-9783846534717\"\u003e\u003ch3\u003eStress Corrosion Cracking of  X-70 Microalloyed steel in  carbonates, chlorides and sulfates solutions\u003c\/h3\u003e\u003c\/div\u003e","brand":"Autorenwelt Shop","offers":[{"title":"Softcover - 9783846534717","offer_id":39471240151133,"sku":"9783846534717","price":49.0,"currency_code":"EUR","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0940\/0622\/files\/9f30bdbe-eca2-43d6-9124-6c2a5bd3c626.jpg?v=1769667334","url":"https:\/\/shop.autorenwelt.de\/en\/products\/stress-corrosion-cracking-of-x-70-steel-in-carbonates-solutions-von-alvaro-torres-sergio-serna-und-bernardo-campillo","provider":"Autorenwelt Shop","version":"1.0","type":"link"}